Laserfiche WebLink
Routine crack filling required <br />Roads show first signs of aging, and they may have very slight ravelling. Any longitudinal cracks are along <br />paving joint. Transverse cracks may be approximately 10 feet apart. All cracks are 1/4" or less with little or <br />no crack erosion. Few if any patches, all in very good condition. <br />Transverse and <br />longitudinal cracks <br />Cracks are tight and sealed <br />Transverse cracks <br />About 10' apart and <br />well sealed <br />Page 57 <br />